Views: 4 Author: Site Editor Publish Time: 2019-10-08 Origin: Site
Breakage at the break
1. The hose is broken at one or more places, and the gap is neat:
The main reason for this phenomenon is that the system pressure is too high, exceeding the pressure resistance of the hose. If the system pressure meets the requirements, check whether the actual pressure resistance of the hose used meets the design requirements.
2. Torsion occurs at the rupture of the hose:
This phenomenon occurs because the hose is excessively twisted during installation or use. After the hose is twisted, the structure of the reinforcing layer changes, the gap between the braided and wound wires increases, and the compressive strength of the hose is lowered, and the hose is easily broken under the action of high pressure. Therefore, during the process of using or storing the hose, the hose should not be subjected to the torsional moment. When installing the hose, the axes of the two joints should be placed on the same plane as much as possible to prevent the hose from being twisted during use.
3. The wire at the rupture of the hose is curled and has obvious necking:
The reason for this phenomenon is that the hose is subjected to excessive tensile deformation, and the layers are separated to reduce the compressive strength. The hose will shrink or elongate in the longitudinal direction under the action of high pressure, and the general expansion and contraction amount is +2% to 4% in the normal state. If the hose is selected too short during installation, it will be greatly stretched during operation, and if it is severe, it will be broken or loose. If the span of the hose is too large, the weight of the hose and the weight of the hose will also be This will give the hose a large tensile force, which can also occur in severe cases. Therefore, appropriate solutions should be adopted depending on the specific situation. If it is too tight during installation, replace the lengthened new tube